1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Hommel Frit 497

Description: Zinc magnesia borosilicate frit

Oxide Analysis Formula Tolerance
K2O 2.00% 0.09
Li2O 1.00% 0.14
MgO 4.00% 0.42
Na2O 2.00% 0.14
ZnO 4.00% 0.21
B2O3 25.00% 1.53
Al2O3 3.00% 0.12
SiO2 59.00% 4.17
Oxide Weight 424.73
Formula Weight 424.73

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 3.70
Frit Softening Point 1100F