Ferro Frit 4616

Description: High zinc borosilicate frit for matte glazes, matte frit 1040-1100C

Oxide Analysis Formula Tolerance
CaO 4.60% 0.15
K2O 1.55% 0.03
Na2O 3.39% 0.10
ZnO 32.04% 0.72
B2O3 10.27% 0.27
Al2O3 4.46% 0.08
SiO2 43.70% 1.33
Oxide Weight 182.94
Formula Weight 182.94

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 4103
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy