Hommel Frit 450

Description: Medium lead low alumina borax frit

Oxide Analysis Formula Tolerance
CaO 5.98% 0.34
K2O 1.80% 0.06
MgO 0.32% 0.03
Na2O 2.36% 0.12
PbO 31.72% 0.45
B2O3 13.76% 0.63
Al2O3 3.50% 0.11
SiO2 40.56% 2.15
Oxide Weight 318.65
Formula Weight 318.65

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3532
Materials Pemco Frit Pb-1931
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.5 x 10-6
Frit Melting Range (C) 1520F