Ferro Frit 3824

Description: Leadless zinc frit

Oxide Analysis Formula Tolerance
CaO 4.50% 0.19
Na2O 9.10% 0.35
ZnO 16.10% 0.47
B2O3 29.10% 0.98
SiO2 41.20% 1.61
Oxide Weight 235.42
Formula Weight 235.42

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Pemco Frit P-1734
Materials Hommel Frit 446
Materials Fusion Frit FZ-16
The champion in our frit melt-off competitition. This frit showcases the amazing fluxing power of boron and zinc working together. It is 15.5% ZnO.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.30
Frit Melting Range (C) 1400F
By Tony Hansen