Ferro Frit 3496

Description: Medium lead zincless for cone 04-2 artware glazes

Oxide Analysis Formula Tolerance
CaO 4.20% 0.27
K2O 1.40% 0.05
Na2O 2.40% 0.14
PbO 33.10% 0.54
B2O3 4.30% 0.22
Al2O3 4.90% 0.17
SiO2 49.70% 2.99
Oxide Weight 361.36
Formula Weight 361.36

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Fusion Frit FL-308
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.10
Frit Melting Range (C) 1450F
By Tony Hansen