Ferro Frit 3482

Description: Medium lead high titanium glaze frit cone 06-02

Oxide Analysis Formula Tolerance
CaO 3.30% 0.21
K2O 3.90% 0.15
Na2O 2.70% 0.16
PbO 29.10% 0.48
TiO2 9.70% 0.44
B2O3 6.00% 0.31
SiO2 43.10% 2.62
F 2.20% 0.42
Oxide Weight 364.76
Formula Weight 364.76

Notes

Ideal for 06-02 matte and artware/hobby glazes because of the Ti.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Pemco Frit Pb-1151
Materials Hommel Frit 334
Materials Hommel Frit 27
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.30
Frit Melting Range (C) 1400F
By Tony Hansen