Hommel Frit 344

Description: Low lead calcium borate frit

Oxide Analysis Formula Tolerance
CaO 10.11% 0.57
K2O 3.03% 0.10
Na2O 1.54% 0.08
PbO 18.04% 0.25
B2O3 8.81% 0.40
Al2O3 5.91% 0.18
SiO2 52.05% 2.72
Oxide Weight 312.82
Formula Weight 312.82

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3509
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.10
Co-efficient of Linear Expansion 7.1 x 10-6 (50-450C)
Frit Softening Point 1600F