Alkatrol W-22535

Oxide Analysis Formula Tolerance
K2O 0.65% 0.04
Na2O 0.65% 0.05
TiO2 0.40% 0.03
Al2O3 20.00% 1.00
SiO2 75.90% 6.44
Fe2O3 0.40% 0.01
LOI 2.00%n/a
Oxide Weight 499.80
Formula Weight 510.00

Notes

This version has lower alklai (and therefore higher PCE), finer particle size, lower specific gravity and bulk density.

Related Information

Links

Materials Alkatrol W-20031
Materials Alkatrol
Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.

Data

Pyrometric Cone Equivalent 19
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy