Ferro Frit 3248

Description: Leadless calcium potassium borosilicate frit

Oxide Analysis Formula Tolerance
CaO 5.20% 0.38
K2O 7.00% 0.31
MgO 1.99% 0.20
Na2O 1.63% 0.11
B2O3 4.70% 0.28
Al2O3 15.10% 0.61
SiO2 64.39% 4.41
Oxide Weight 412.12
Formula Weight 412.12

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.60
Frit Melting Range (C) 1900F