Ferro Frit 3227

Alternate Names: F3227 Frit, F3227

Description: Low melting bonding frit used in metals industry

Oxide Analysis Formula Tolerance
K2O 4.10% 0.16
Na2O 13.90% 0.84
B2O3 28.50% 1.53
Al2O3 15.60% 0.57
SiO2 37.90% 2.36
Oxide Weight 373.53
Formula Weight 373.53

Related Information

Links

Materials Fusion Frit F-395
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3221
Materials Ferro Frit 90 741 F
Materials Ferro Frit 90 742 F
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Typecodes Bonding Frits
Also called glass frits, these melt at very low temperatures (e.g. 500C). They are used to bond together materials that can withstand some heat (e.g. abrasives, ceramics, non-oxide ceramics, metals). And as a surface-smoothing agent. The main product properties are melting temperature and thermal expansion. The powders are mixed with binders, applied and then heated up and down to create the bond.

Data

Co-efficient of Linear Expansion 9.8
Frit Melting Range (C) 1300F
By Tony Hansen