Ferro Frit 3226

Description: Leadless vitrified bonded abrasives frit

Oxide Analysis Formula Tolerance
CaO 2.90% 0.31
Na2O 7.30% 0.69
B2O3 36.30% 3.08
Al2O3 1.00% 0.06
SiO2 52.50% 5.16
Oxide Weight 590.20
Formula Weight 590.20

Related Information

Links

Materials Fusion Frit F-245
Materials General Frit GF-143
Materials Ferro Frit 3185
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 2GF241A
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.30
Frit Melting Range (C) 1450F