Hommel Frit 2GF176D

Description: LEADED

Oxide Analysis Formula Tolerance
CaO 5.25% 0.34
K2O 2.03% 0.08
Na2O 1.76% 0.10
PbO 29.83% 0.48
ZrO2 1.18% 0.03
B2O3 11.93% 0.62
Al2O3 3.12% 0.11
SiO2 41.37% 2.48
F 3.53% 0.67
Oxide Weight 360.79
Formula Weight 360.79

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy