Vantage WT Ball Clay

Oxide Analysis Formula Tolerance
SiO2 59.00% 4.01
Al2O3 25.00% 1.00
TiO2 1.20% 0.06
Fe2O3 2.40% 0.06
CaO 0.30% 0.02
MgO 0.70% 0.07
K2O 2.90% 0.13
Na2O 0.20% 0.01
LOI 8.20%n/a
Oxide Weight 374.14
Formula Weight 407.56

Notes

The data sheet describes this as a ball clay designed to produce increased strength and plasticity in plastic forming and extrusion operations. VANTAGE clays are easily dispersed in water for direct slip make down by blunging. They are ideal for use in slurries, filter pressing and extrusion processes, mulling prior to extrusion, and spray drying. In all applications, the rapid pick up and equilibration of process fluids with these clays help minimize batching and blending time.

The VANTAGE series of ball clays are mined and processed under rigid Covia QIPSM statistical quality assurance programs. The result is consistent mineralogy, chemical and physical properties, predictable results in demanding refractory applications.

Related Information

Links

URLs https://digitalfire.com/4sight/datasheets/VantageBallClay.pdf
Covia Vantage Ball Clay data sheet
Materials Vantage RD Ball Clay

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy