Vantage RD Ball Clay

Oxide Analysis Formula Tolerance
Al2O3 65.00% 1.00
SiO2 16.50% 0.43
TiO2 0.90% 0.02
Fe2O3 7.50% 0.07
CaO 0.30% 0.01
MgO 1.00% 0.04
K2O 2.50% 0.04
Na2O 0.80% 0.02
LOI 5.50%n/a
Oxide Weight 148.29
Formula Weight 156.92

Notes

This shares the same data sheet as WT Ball Clay. But their chemistries are very different (this having much lower Al2O3 and really high Fe2O3, thus obviously red burning). Perhaps the "RD" means "Red" and "WT" means "White".

Related Information

Links

URLs https://digitalfire.com/4sight/datasheets/VantageBallClay.pdf
Covia Vantage Ball Clay data sheet
Materials Vantage WT Ball Clay

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy