General Frit GF-46

Description: Medium lead boron frit

Oxide Analysis Formula Tolerance
K2O 1.40% 0.04
Na2O 4.30% 0.21
CaO 7.30% 0.39
PbO 25.90% 0.35
Al2O3 2.20% 0.07
B2O3 16.30% 0.71
SiO2 42.60% 2.15
Oxide Weight 302.68
Formula Weight 302.68