General Frit GF-30

Description: Low lead high boron frit

Oxide Analysis Formula Tolerance
K2O 1.50% 0.11
Na2O 2.60% 0.28
CaO 0.90% 0.11
PbO 16.40% 0.50
Al2O3 7.10% 0.47
B2O3 30.90% 3.01
SiO2 40.50% 4.57
Oxide Weight 677.85
Formula Weight 677.85

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.