1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Laguna Spodumene Substitute

Oxide Analysis Formula Tolerance
Li2O 7.10% 0.94
K2O 0.60% 0.03
Na2O 0.30% 0.02
P2O5 0.40% 0.01
Al2O3 25.00% 0.97
Fe2O3 0.15% -
MnO2 0.06% -
SiO2 66.20% 4.37
LOI 0.20%n/a
Oxide Weight 395.63
Formula Weight 396.42

Related Information

Links

Materials Spodumene
Spodumene is a lithium sourcing feldspar, an alternative to lithium carbonate to supply Li2O to ceramic glazes. Contains up to about 8% Li2O.