Description: Ancienne fritte
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 8.84% | 0.37 | |
| MgO | 0.03% | - | |
| K2O | 8.68% | 0.21 | |
| Na2O | 11.13% | 0.42 | |
| Al2O3 | 9.00% | 0.21 | |
| B2O3 | 13.55% | 0.45 | |
| SiO2 | 48.76% | 1.89 | |
| Oxide Weight | 232.55 | ||
| Formula Weight | 232.55 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |