Moulin Fritte M2

Description: Ancienne fritte

Oxide Analysis Formula Tolerance
CaO 8.24% 0.44
K2O 3.97% 0.13
Na2O 9.11% 0.44
Al2O3 7.25% 0.21
B2O3 17.19% 0.74
SiO2 54.25% 2.69
Oxide Weight 297.68
Formula Weight 297.68

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.