G2934 Base

Description: Cone 6 matte base glaze

Oxide Analysis Formula Tolerance
CaO 9.77% 0.54
MgO 5.06% 0.39
K2O 0.19% 0.01
Na2O 1.23% 0.06
B2O3 1.23% 0.05
Al2O3 14.85% 0.45
SiO2 52.42% 2.71
Fe2O3 0.14% -
LOI 14.00%n/a
Oxide Weight 263.99
Formula Weight 306.96

Notes

Clear base sold as a powder by Plainsman Clays. The recipe and usage of G2934 are well documented online.