Description: Cone 6 glossy base glaze
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 5.00% | 0.48 | |
| K2O | 0.88% | 0.05 | |
| MgO | 0.72% | 0.10 | |
| Na2O | 4.26% | 0.37 | |
| B2O3 | 5.63% | 0.44 | |
| Al2O3 | 11.74% | 0.62 | |
| SiO2 | 68.62% | 6.17 | |
| LOI | 3.00% | n/a | |
| Oxide Weight | 523.39 | ||
| Formula Weight | 539.58 | ||
Clear base sold as a powder by Plainsman Clays. The recipe and usage of G2926B are well documented online.