Colorobbia Frit VSA-7000

Oxide Analysis Formula Tolerance
SiO2 51.00% 2.24
Al2O3 13.00% 0.34
B2O3 12.00% 0.45
Na2O 16.00% 0.68
K2O 3.00% 0.08
CaO 5.00% 0.24
Oxide Weight 263.83
Formula Weight 263.83