Frit 268-D

Alternate Names: Frit FB-268-D

Description: Zircon unleadled frit

Oxide Analysis Formula Tolerance
SiO2 42.50% 2.27 2.5
B2O3 12.50% 0.58 2.5
Na2O 12.50% 0.65 2.5
K2O 7.50% 0.26 2.5
CaO 1.00% 0.06 1
Al2O3 7.50% 0.24 2.5
ZrO2 7.50% 0.20 2.5
ZnO 1.00% 0.04 1
F 2.50% 0.42 2.5
Oxide Weight 303.53
Formula Weight 303.53

Notes

FRIT ID F2 SIO2 B2O3 Na2O K2O CaO Al2O3 ZrO2 ZnO CTE
FB268-D-2 1-5 40-45 10-15 10-15 5-10 0-2 5-10 10-15 0-2 10.06

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Fusion Frit FZ-10
Materials Hommel Frit 472
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Typecodes Available from Laguna Clays

Data

Co-efficient of Linear Expansion 10.06

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy