Ferro Frit 3389

Oxide Analysis Formula Tolerance
Na2O 6.34% 0.40
K2O 2.41% 0.10
CaO 7.17% 0.50
Al2O3 7.82% 0.30
SiO2 69.14% 4.50
B2O3 7.12% 0.40
Oxide Weight 391.16
Formula Weight 391.16