Description: Zircon frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 3.84% | 0.40 | |
| K2O | 4.62% | 0.29 | |
| Al2O3 | 8.75% | 0.50 | |
| Na2O | 2.28% | 0.21 | |
| Li2O | 0.51% | 0.10 | |
| B2O3 | 18.77% | 1.57 | |
| SiO2 | 51.86% | 5.03 | |
| ZrO2 | 9.36% | 0.44 | |
| Oxide Weight | 583.43 | ||
| Formula Weight | 583.43 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |