Mondre and Manz Frit M9358

Description: Calcium alkaline leadless high borax frit

Oxide Analysis Formula Tolerance
K2O 6.27% 0.14
CaO 14.94% 0.54
ZnO 3.10% 0.08
MgO 0.57% 0.03
Na2O 6.49% 0.21
Al2O3 13.58% 0.27
B2O3 26.48% 0.78
SiO2 28.58% 0.97
Oxide Weight 204.20
Formula Weight 204.20

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.