Sodium Feldspar 1210

Description: Turkish Feldspar

Oxide Analysis Formula Tolerance
SiO2 67.10% 6.02
TiO2 0.02% -
Al2O3 19.20% 1.02
Fe2O3 0.04% -
Na2O 8.40% 0.73
K2O 4.70% 0.27
LOI 0.10%n/a
Oxide Weight 536.53
Formula Weight 537.06

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.
URLs http://ceramics.sibelcotools.com/tiles/porcelain-tiles/feldspar/
Sibelco Feldspar data