Colorobbia Frit 250

Description: High zinc opacified frit

Oxide Analysis Formula Tolerance
ZnO 11.43% 0.34
Al2O3 6.99% 0.17
ZrO2 9.78% 0.19
MgO 2.35% 0.14
Na2O 0.56% 0.02
SiO2 55.40% 2.24
K2O 4.02% 0.10
Fe2O3 0.13% -
CaO 9.05% 0.39
TiO2 0.08% -
LOI 0.11%n/a
Oxide Weight 242.35
Formula Weight 242.62

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.