Torrecid Frit 31056

Description: High zinc opacified frit

Oxide Analysis Formula Tolerance
ZnO 10.48% 0.29
MgO 2.11% 0.12
ZrO2 7.55% 0.14
Al2O3 6.89% 0.15
Fe2O3 0.11% -
K2O 5.26% 0.13
TiO2 0.08% -
Na2O 0.21% 0.01
SiO2 55.06% 2.08
CaO 11.19% 0.45
LOI 0.99%n/a
Oxide Weight 224.97
Formula Weight 227.22

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.