Esmalglass Frit FT2803

Oxide Analysis Formula Tolerance
SiO2 60.00% 1.97
Na2O 0.40% 0.01
P2O5 0.10% -
CaO 13.80% 0.48
ZrO2 0.40% 0.01
Fe2O3 0.10% -
K2O 5.00% 0.10
MgO 2.80% 0.14
Al2O3 5.10% 0.10
ZnO 10.70% 0.26
PbO 0.10% -
LOI 0.40%n/a
Oxide Weight 194.05
Formula Weight 194.83

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 1140C
Frit Melting Range (C) 1325C
By Tony Hansen