Potclays Frit 2263

Alternate Names: 2263 Standard boraksfritte, Potclays Standard Borax Frit

Description: High calcium borosilicate frit

Oxide Analysis Formula Tolerance
CaO 15.22% 0.63
K2O 1.33% 0.03
MgO 0.05% -
Na2O 8.75% 0.33
B2O3 18.76% 0.63
Al2O3 7.55% 0.17
SiO2 48.34% 1.88
Oxide Weight 233.76
Formula Weight 233.76

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit CC-250
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.