Esmalglass Frit FO 963

Oxide Analysis Formula Tolerance
K2O 5.20% 0.12
CaO 10.20% 0.39
Al2O3 5.60% 0.12
Fe2O3 0.10% -
ZrO2 7.60% 0.13
Na2O 0.50% 0.02
ZnO 10.70% 0.28
SiO2 56.60% 2.02
MgO 3.60% 0.19
Oxide Weight 214.87
Formula Weight 214.87

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 940C
Frit Melting Range (C) 1170C
By Tony Hansen