Keramikos Bariumzink Fritte

Description: Barium zinc frit

Oxide Analysis Formula Tolerance
BaO 35.63% 0.50
ZnO 18.92% 0.50
Al2O3 5.22% 0.11
SiO2 40.23% 1.44
Oxide Weight 215.12
Formula Weight 215.12

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.