Description: Zink Fritte, Zinc frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| B2O3 | 11.45% | 0.30 | |
| SiO2 | 46.25% | 1.41 | |
| CaO | 2.98% | 0.10 | |
| K2O | 5.00% | 0.10 | |
| Na2O | 4.94% | 0.15 | |
| ZnO | 29.38% | 0.66 | |
| Oxide Weight | 182.88 | ||
| Formula Weight | 182.88 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |