V15098

Alternate Names: V 15098,V-15098

Description: Alkali-Zink-Bor

Oxide Analysis Formula Tolerance
CaO 0.28% 0.41
K2O 0.35% 0.31
ZnO 0.28% 0.28
B2O3 0.16% 0.19
SiO2 3.16% 4.33
Oxide Weight 348.25
Formula Weight 348.25

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 70
Frit Softening Point 655C