M136

Alternate Names: M 136,M-136

Description: Natriubor-Silikat

Oxide Analysis Formula Tolerance
PbO 0.45% 0.17
CaO 0.45% 0.69
K2O 0.15% 0.14
B2O3 0.45% 0.56
Al2O3 0.15% 0.13
SiO2 1.75% 2.50
Oxide Weight 292.35
Formula Weight 292.35

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 67
Frit Softening Point 603C