1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Frit 35.108

Alternate Names: 35 108,35-108

Oxide Analysis Formula Tolerance
Na2O 2.41% 0.14
CaO 4.20% 0.27
PbO 33.40% 0.54
K2O 1.31% 0.05
B2O3 4.24% 0.22
Al2O3 4.81% 0.17
SiO2 49.64% 2.98
Oxide Weight 360.68
Formula Weight 360.68

Related Information

Data

Frit Melting Range (C) 920-1080C