1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Frit 35.320

Alternate Names: Frit 35 320, Frit 35-320

Oxide Analysis Formula Tolerance
PbO 55.51% 0.52
BaO 35.07% 0.48
SiO2 9.42% 0.33
Oxide Weight 209.44
Formula Weight 209.44

Related Information

Data

Frit Melting Range (C) 800-1080C