Alternate Names: Frit 34 030, Frit 34-030
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| PbO | 68.01% | 0.94 | |
| K2O | 1.22% | 0.04 | ` |
| Na2O | 0.40% | 0.02 | |
| Al2O3 | 2.31% | 0.07 | |
| SiO2 | 28.05% | 1.44 | |
| Oxide Weight | 308.51 | ||
| Formula Weight | 308.51 | ||
| Frit Melting Range (C) | 900-1080C |
|---|