Moulin Fritte M44

Description: Fritte ua baryum

Oxide Analysis Formula Tolerance
BaO 39.75% 1.00
Al2O3 13.49% 0.51
SiO2 46.76% 3.00
Oxide Weight 385.66
Formula Weight 385.66

Notes

Corrected this wrong analysis Oct 2022:
BaO 47.0, Al2O3 16.0, SiO2 37.0

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin

Data

Frit Softening Point 855C