Moulin Fritte M864

Description: Fritte Raku

Oxide Analysis Formula Tolerance
Na2O 15.61% 1.00
Al2O3 5.14% 0.20
B2O3 26.29% 1.50
SiO2 52.96% 3.50
Oxide Weight 397.18
Formula Weight 397.18

Notes

Corrected chemistry of this frit Oct 2022, it was:
BaO 26.3, Na2O 15.6, Al2O3 5.1, SiO2 53.0

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin

Data

Frit Softening Point 565C