Frit 1818

Description: Alkali calcium aluminun silicate frit

Oxide Analysis Formula Tolerance
CaO 12.58% 0.33
K2O 4.04% 0.06
MgO 0.69% 0.03
Na2O 23.92% 0.58
TiO2 0.03% -
Al2O3 7.75% 0.11
P2O5 0.01% -
SiO2 50.58% 1.26
Fe2O3 0.40% -
Oxide Weight 149.23
Formula Weight 149.23

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.