Alternate Names: 37 06,37-06
Description: Bleifreie Barium-Fritte
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 47.00% | 1.00 | |
| Al2O3 | 17.00% | 0.54 | |
| SiO2 | 36.00% | 1.95 | |
| Oxide Weight | 326.17 | ||
| Formula Weight | 326.17 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 70 x 10-7 |
|---|---|
| Frit Melting Range (C) | 1180-1280C |