Glasurfritten 37.024

Alternate Names: 37 024,37-024

Description: Bleifreie Alkali-Fritte

Oxide Analysis Formula Tolerance
CaO 3.00% 0.11
K2O 2.00% 0.04
Na2O 19.00% 0.64
ZnO 8.00% 0.20
Al2O3 2.00% 0.04
SiO2 66.00% 2.29
Oxide Weight 208.58
Formula Weight 208.58

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 110x10-7
Frit Softening Point 565C
Frit Melting Range (C) 980-1060C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy