Description: Alkaline Borate Frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 2.30% | 0.06 | |
| Na2O | 15.71% | 0.65 | |
| CaO | 6.27% | 0.29 | |
| Al2O3 | 3.70% | 0.09 | |
| B2O3 | 2.58% | 0.10 | |
| SiO2 | 69.44% | 2.97 | |
| Oxide Weight | 256.69 | ||
| Formula Weight | 256.69 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Frit Melting Range (C) | 900-1000C |
|---|