1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ferro Richoux Frit 21 C006

Description: Alkaline Borate Frit

Oxide Analysis Formula Tolerance
K2O 0.99% 0.03
Na2O 19.17% 0.76
CaO 4.77% 0.21
Al2O3 11.51% 0.28
B2O3 10.74% 0.38
SiO2 52.82% 2.17
Oxide Weight 247.08
Formula Weight 247.08

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Melting Range (C) 850-1000C