IMCO KPW Clay

Oxide Analysis Formula Tolerance
CaO 0.02% -
K2O 3.20% 0.14
MgO 0.47% 0.05
Al2O3 25.20% 1.00
SiO2 61.20% 4.12
Fe2O3 1.74% 0.04
TiO2 1.04% 0.05
Na2O 0.16% 0.01
LOI 11.00%n/a
Oxide Weight 376.55
Formula Weight 423.09

Notes

Manufacturer says: A nice white clay in the raw state. Fires to a cream color.

Physical data can be found on the link to the product information web page of the manufacturer.

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
URLs https://www.clayimco.com/industrial-clays
IMCO information on their mined clays

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy