Podmore Frit P2250

Description: High alkali frit

Oxide Analysis Formula Tolerance
CaO 6.31% 0.20
K2O 15.90% 0.30
SiO2 50.71% 1.50
Na2O 17.44% 0.50
Al2O3 5.74% 0.10
B2O3 3.91% 0.10
Oxide Weight 177.78
Formula Weight 177.78

Notes

Made by Podmore and Sons
Formerly Frit T

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Potclays Frit 2275
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.