Frit A 3129

Description: Reimbold & Strick stoneware matte frit

Oxide Analysis Formula Tolerance
PbO 45.00% 0.37
ZnO 25.00% 0.56
Al2O3 3.00% 0.05
CaO 1.00% 0.03
K2O 2.00% 0.04
SiO2 24.00% 0.73
Oxide Weight 182.55
Formula Weight 182.55

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.reimbold-und-strick.de/images/pdf/keramisch.pdf
Reimbold & Strick Frit chart with chemistry

Data

Co-efficient of Linear Expansion 62 x 10-7 (20-400C)
Frit Softening Point 560C
Glass Transition Temperature 490C