Frit VO 6079

Description: Reimbold & Strick opacified stoneware opaque frit

Oxide Analysis Formula Tolerance
Al2O3 7.00% 0.32
CaO 6.00% 0.50
B2O3 13.00% 0.87
ZrO2 12.00% 0.45
K2O 1.00% 0.05
Na2O 6.00% 0.45
SiO2 55.00% 4.27
Oxide Weight 466.54
Formula Weight 466.54

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.reimbold-und-strick.de/images/pdf/keramisch.pdf
Reimbold & Strick Frit chart with chemistry

Data

Co-efficient of Linear Expansion 58 x 10-7 (20-400C)
Frit Softening Point 670C
Glass Transition Temperature 600C